Cart 0

NG-10-R01 Welding Procedures on Base-Metal Cracking Adjacent to Girth Welds and Welded Connections

$50.00

The objectives of this work were to investigate welding techniques that would insure against base-metal cracks in the heat-affected zones of girth welds.