{"product_id":"l51748-detection-of-stress-corrosion-induced-toe-cracks-advancement-of-the-developed-technique-1","title":"L51748 Detection of Stress Corrosion Induced Toe Cracks-Advancement of the Developed Technique","description":"\u003cp\u003eIn the past few years an ongoing problem has existed with stress corrosion cracking (SCC) in pipelines around the world. Several member companies of the Pipeline Research Council International, Inc. have experienced multiple incidents as a result of ERW defects and SCC. TCPL is running a series of hydrostatic tests and trial digs to identify the most severely affected areas. These excavations and failure studies have ascertained that most of the SCC causing failure has been on the outside diameter of long seam welded pipe at the edge of the weld. Defects at that location are known as \"Toe-Cracks\"\u003c\/p\u003e\n\n\u003cp\u003eGinzel has developed an ultrasonic inspection technique that will detect both SCC colonies and toe cracks in long seam pipe. The main design objective for this research project was the selection and placement of ultrasonic transducers to combine weld, plate thickness and lamination inspection, along with SCC detection and sizing. Examination of sample pipe sections to demonstrate its success is reported.\u003c\/p\u003e\n\n\u003cp\u003eThe primary stages for this research project are:\u003c\/p\u003e\n\n\n\t\u003cp\u003e Assemble test equipment\u003cbr\u003e\n\tEstablish test procedure\u003cbr\u003e\n\tSystem trials and data collection\u003cbr\u003e\n\tEvaluation of system performance and collected data\u003cbr\u003e\n\tCorrelation of test data - Results\u003c\/p\u003e","brand":"PRCI Store","offers":[{"title":"Default Title","offer_id":44367593373774,"sku":"18565","price":395.0,"currency_code":"USD","in_stock":true}],"url":"https:\/\/prci-store.myshopify.com\/products\/l51748-detection-of-stress-corrosion-induced-toe-cracks-advancement-of-the-developed-technique-1","provider":"PRCI Store","version":"1.0","type":"link"}