{"product_id":"l51928-integrity-and-remaining-life-of-pipe-with-stress-corrosion-cracking-1","title":"L51928 Integrity and Remaining Life of Pipe with Stress Corrosion Cracking","description":"\u003cp\u003eThe CorLAS computer program for corrosion life assessment of piping and pressure vessels was found to provide very good predictions of actual SCC failure conditions, but it gave somewhat conservative predictions for very long cracks. This research project was undertaken to develop improvements to CorLAS.\u003c\/p\u003e","brand":"PRCI Store","offers":[{"title":"Default Title","offer_id":44367594618958,"sku":"18515","price":995.0,"currency_code":"USD","in_stock":true}],"url":"https:\/\/prci-store.myshopify.com\/products\/l51928-integrity-and-remaining-life-of-pipe-with-stress-corrosion-cracking-1","provider":"PRCI Store","version":"1.0","type":"link"}