{"product_id":"pr-460-134506-r01-development-of-a-modern-assessment-method-for-longitudinal-seam-weld-cracks","title":"PR-460-134506-R01 Development of a Modern Assessment Method for Longitudinal Seam Weld Cracks","description":"\u003cp\u003eThis research effort was aimed at developing a state-of-the-art fracture model for pipelines with longitudinal seam weld cracks. Approximately 200 finite element simulations were performed, and the results were fit to a parametric equation. The report contains the theoretical framework of the model, a description of the finite element study, and a set of tables that contain fitting constants for the model. The benefit of this research is the creation of a significantly more accurate model to predict burst pressure of pipes with longitudinal seam weld flaws. Increased accuracy in predictions will improve the integrity of seam welded pipe.\u003c\/p\u003e","brand":"PRCI Store","offers":[{"title":"Default Title","offer_id":44367601926222,"sku":"18343","price":950.0,"currency_code":"USD","in_stock":true}],"url":"https:\/\/prci-store.myshopify.com\/products\/pr-460-134506-r01-development-of-a-modern-assessment-method-for-longitudinal-seam-weld-cracks","provider":"PRCI Store","version":"1.0","type":"link"}